We have measured the excitation and emission energy dependence of the lifetimes of the 2.7 eV photoluminescence band associated to oxygen deficient centers in silica glasses. The non-exponential behavior of this time decay is consistent with intrinsic conformational heterogeneity of these point defects in the amorphous matrix. Accordingly, we have analyzed the data in terms of a radiative rates distribution. Moreover, both surface and bulk typologies of these point defects have been studied. The mean value of the lifetime distribution of the surface defects increases from 12 to 15 ms varying the excitation energy from 4.6 to 5.2 eV, and it increases from 14 to 15 ms in the emission energy interval between 2.6 and 3.0 eV. As well similar variations of the lifetime are observed for interior defects, when measured at different excitation and emission energies. We can also estimate the width of the lifetime distribution of this ensemble of point defects in silica glass.
D'Amico, M., Leone, M. (2008). Conformational heterogeneity of the point defects in silica: The lifetime of the phosphorescence band at 2.7 eV. JOURNAL OF NON-CRYSTALLINE SOLIDS, 354(2-9), 239-243 [10.1016/j.jnoncrysol.2007.06.081].
Conformational heterogeneity of the point defects in silica: The lifetime of the phosphorescence band at 2.7 eV
D'AMICO, Michele;LEONE, Maurizio
2008-01-01
Abstract
We have measured the excitation and emission energy dependence of the lifetimes of the 2.7 eV photoluminescence band associated to oxygen deficient centers in silica glasses. The non-exponential behavior of this time decay is consistent with intrinsic conformational heterogeneity of these point defects in the amorphous matrix. Accordingly, we have analyzed the data in terms of a radiative rates distribution. Moreover, both surface and bulk typologies of these point defects have been studied. The mean value of the lifetime distribution of the surface defects increases from 12 to 15 ms varying the excitation energy from 4.6 to 5.2 eV, and it increases from 14 to 15 ms in the emission energy interval between 2.6 and 3.0 eV. As well similar variations of the lifetime are observed for interior defects, when measured at different excitation and emission energies. We can also estimate the width of the lifetime distribution of this ensemble of point defects in silica glass.File | Dimensione | Formato | |
---|---|---|---|
2008_JNCS_354_239.pdf
Solo gestori archvio
Descrizione: Articolo
Dimensione
499.26 kB
Formato
Adobe PDF
|
499.26 kB | Adobe PDF | Visualizza/Apri Richiedi una copia |
I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.